Ask three tarpaulin suppliers what holds their product together and you will get the same answer: the base fabric. They are right — and they are describing one specific kind of base fabric. The PVC tarpaulin industry has standardized on woven and warp-knitted polyester, and for heavy truck covers and long-term industrial covers that choice is earned. But it is not the only construction that works, and for a large share of what is sold as “tarpaulin” today — printed banners, light awnings, temporary covers, folding and rolled goods — a laid scrim core does the same structural job at a fraction of the weight.
This guide explains how the sandwich works, why woven became the default, where a laid scrim earns its place — and, just as importantly, where it does not.
Every PVC tarpaulin is a three-layer composite: a PVC layer, a reinforcing fabric in the middle, and another PVC layer. The division of labor is clean. The PVC delivers waterproofing, UV resistance, mildew and chemical protection; the fabric core carries the mechanical load — tensile strength, tear resistance and dimensional stability.
Tear Logic: In a plain film, a puncture follows the line of least resistance and keeps running. A grid interrupts that path: the threads of the core stop a small puncture from becoming a long rip. Any open-grid reinforcement, woven or not, buys this behavior.
The mainstream core is a woven or warp-knitted polyester fabric, with finished goods running roughly 500–900 g/m² and tensile values in the thousands of N/5cm (industry-published reference values, e.g. Botai’s laminated tarpaulin tables).
If your product is a 900 g/m² truck cover guaranteed for years of highway service, the woven core is the right answer.
A laid scrim is a chemically bonded, non-woven grid of continuous filaments. It is dramatically lighter (2 to 10 g/m²) while forming the same continuous grid that interrupts tear paths.
Lighter, more drapable, and flatter surface for superior print quality.
Withstands repeated folding and conforms to curves without cracking at crease lines.
Carries the load of wind flutter and handling without unnecessary dead weight.
Supplied up to 2,500 mm wide to reduce seams, the primary failure point.
In PVC and LVT flooring, the same low-elongation grid principle keeps large-format goods flat through thermal cycling.
| Application | Recommended construction | Grammage | Why this grid |
|---|---|---|---|
| Printed banner / signage media | CP8*12PH | 2–2.5 g/m² | Lightest core; print drape and handling dominate |
| Light awning / temporary cover | CP2.5*10PH | 4–5 g/m² | Balanced MD strength for flutter and roll-up service |
| General tarpaulin / bag / liner | CP2.5*5PH | 5.5–6 g/m² | Denser grid for tear-path interruption at low weight |
| Sail cloth / demanding flex service | CP4*6PH | 7.8–10 g/m² | Heavier grid where folding fatigue is the failure mode |
| Heavy truck cover / long-term industrial | woven base fabric (industry standard) | 500–900 g/m² finished | Four-figure tensile absolutes |
| Product | Mesh | Grammage | Yarn | Fits | Page |
|---|---|---|---|---|---|
| CP4*4PH | 4×4 /cm | per datasheet | Polyester 1100 dtex | Advertising banner, tarpaulin, sail cloth, automotive | CP4*4PH |
| CP4*6PH | 4×6 mm | 7.8–10 g/m² | Polyester | Sail cloth, flex-demanding covers | Datasheet |
| CP2.5*10PH | 2.5×10 mm | 4–5 g/m² | Polyester | Light awning, temporary covers | same data sheet |
| CP8*12PH | 8×12.5 mm | 2–2.5 g/m² | Polyester | Banner media, lightest builds | same data sheet |
| PVC Tarpaulin Laminated | scrim-laminated build | heavy-duty | Polyester scrim core | Finished-goods direction: truck, machinery, stockpile | Product Page |


Process notes: Whether your line is knife coating, hot-melt or two-step hot lamination, the scrim’s binder must match the coating chemistry and the 160–190 °C process window typical of PVC coating. For the adhesive-facing version, see our tape scrim and binder-matching guide.
Send us this for a tailored recommendation:
Can a laid scrim completely replace a woven base fabric?
No. Heavy, long-service covers stay woven territory. Laid scrim excels where weight, drape, and print surface dominate.
Is a lighter scrim always cheaper once laminated?
Usually on material, but cost per qualified finished roll is the honest metric. Start from the load, then trim weight.
Will the grid interfere with welding seams?
Welding fuses the PVC skins; the grid sits inside the bond line. Seam behavior depends on grid density and coating formulation.
Can mesh size and grammage be customized?
Yes. Grid densities from 0.8 to 3 yarns/cm, square or tri-directional, and custom binder systems are available.
Ready to optimize your production?